Thule (Thule) is recalling certain Thule Range, Camber 2, and Camber 4 bike carriers. The weld on the on the bike arm assembly may be defective, causing the bike arm assembly to detach.
Thule – Bike Arm Assembly Weld Defect
| Report Received Date | 10/21/2022 |
| NHTSA ID | 22E091000 |
| Consequence Summary | A detached bike arm assembly can fall into the roadway, increasing the risk of a crash. |
| Corrective Action | Thule will replace the bike mast assembly, free of charge. Owner notification letters were mailed November 9, 2022. Owners may contact Thule customer service at 1-888-290-1266, by e-mail at rangecamber22@thule.com, or at www.thule.com/ rangecamber22recall. |
| Recall Code | NR (Not Reported) |
| Potentially Affected | 4759 |
| Fire Risk When Parked | No |
| Do Not Drive | No |
| Recall Link | Go to Recall (https://www.nhtsa.gov/recalls?nhtsaId=22E091000) |