Porsche Cars North America (Porsche) is recalling certain 2015 Porsche 918 Spyder vehicles. The connecting shafts of the longitudinal and transverse control arms may fail due to stress corrosion cracking, impacting vehicle handling.
Porsche Cars North America – Stress Corrosion Cracking of Control Arm Shafts
| Report Received Date | 05/03/2018 |
| NHTSA ID | 18V287000 |
| Consequence Summary | If the control arm connecting shafts crack, affecting vehicle handling, it can increase the risk of a crash. |
| Corrective Action | Porsche will notify owners, and dealers will replace the longitudinal and transverse control arms, free of charge. The recall began on September 6, 2018. Owners may contact Porsche customer service at 1-800-767-7243. Porsche's number for this recall is AJ04. |
| Recall Code | AJ04 |
| Potentially Affected | 305 |
| Fire Risk When Parked | No |
| Do Not Drive | No |
| Recall Link | Go to Recall (https://www.nhtsa.gov/recalls?nhtsaId=18V287000) |