Porsche Cars North America (Porsche) is recalling certain 2015 Porsche 918 Spyder vehicles. The connecting shafts of the longitudinal and transverse control arms may fail due to stress corrosion cracking, impacting vehicle handling.
Porsche Cars North America (Porsche) is recalling certain 2015 Porsche 918 Spyder vehicles. The connecting shafts of the longitudinal and transverse control arms may fail due to stress corrosion cracking, impacting vehicle handling.